Lexan PC DMX9455物性
改良的抗刮伤性能,标准的流动性,耐燃性V0/1.5mm, 仅有不透明颜色.
Property
| TYPICAL PROPERTIES (1) | ||||
| 
			 MECHANICAL 
			 | 
			Value | Unit | Standard | |
| 
			 Tensile Stress, yld, Type I, 50 mm/min 
			 | 
			
			 810 
			 | 
			
			 kgf/cm2 
			 | 
			
			 ASTM D 638 
			 | 
		|
| 
			 Tensile Stress, brk, Type I, 50 mm/min 
			 | 
			
			 660 
			 | 
			
			 kgf/cm2 
			 | 
			
			 ASTM D 638 
			 | 
		|
| 
			 Tensile Strain, yld, Type I, 50 mm/min 
			 | 
			
			 7 
			 | 
			
			 % 
			 | 
			
			 ASTM D 638 
			 | 
		|
| 
			 Tensile Strain, brk, Type I, 50 mm/min 
			 | 
			
			 70 
			 | 
			
			 % 
			 | 
			
			 ASTM D 638 
			 | 
		|
| 
			 Tensile Modulus, 50 mm/min 
			 | 
			
			 29500 
			 | 
			
			 kgf/cm2 
			 | 
			
			 ASTM D 638 
			 | 
		|
| 
			 Flexural Stress, yld, 1.3 mm/min, 50 mm span 
			 | 
			
			 1220 
			 | 
			
			 kgf/cm2 
			 | 
			
			 ASTM D 790 
			 | 
		|
| 
			 Flexural Modulus, 1.3 mm/min, 50 mm span 
			 | 
			
			 26500 
			 | 
			
			 kgf/cm2 
			 | 
			
			 ASTM D 790 
			 | 
		|
| 
			 Hardness, Rockwell L 
			 | 
			
			 108 
			 | 
			
			 - 
			 | 
			
			 ASTM D 785 
			 | 
		|
| 
			 Hardness, Rockwell M 
			 | 
			
			 93 
			 | 
			
			 - 
			 | 
			
			 ASTM D 785 
			 | 
		|
| 
			 Taber Abrasion, CS-17, 1 kg 
			 | 
			
			 10 
			 | 
			
			 mg/1000cy 
			 | 
			
			 ASTM D 1044 
			 | 
		|
| 
			 Taber Abrasion, CS-17, 1 kg 
			 | 
			
			 10 
			 | 
			
			 mg/1000cy 
			 | 
			
			 SABIC Method 
			 | 
		|
| 
			 Tensile Stress, yield, 50 mm/min 
			 | 
			
			 80 
			 | 
			
			 MPa 
			 | 
			
			 ISO 527 
			 | 
		|
| 
			 Tensile Stress, break, 50 mm/min 
			 | 
			
			 60 
			 | 
			
			 MPa 
			 | 
			
			 ISO 527 
			 | 
		|
| 
			 Tensile Strain, yield, 50 mm/min 
			 | 
			
			 7 
			 | 
			
			 % 
			 | 
			
			 ISO 527 
			 | 
		|
| 
			 Tensile Strain, break, 50 mm/min 
			 | 
			
			 40 
			 | 
			
			 % 
			 | 
			
			 ISO 527 
			 | 
		|
| 
			 Tensile Modulus, 1 mm/min 
			 | 
			
			 2450 
			 | 
			
			 MPa 
			 | 
			
			 ISO 527 
			 | 
		|
| 
			 Flexural Stress, yield, 2 mm/min 
			 | 
			
			 108 
			 | 
			
			 MPa 
			 | 
			
			 ISO 178 
			 | 
		|
| 
			 Flexural Modulus, 2 mm/min 
			 | 
			
			 2450 
			 | 
			
			 MPa 
			 | 
			
			 ISO 178 
			 | 
		|
| 
			 Hardness, H358/30 
			 | 
			
			 128 
			 | 
			
			 MPa 
			 | 
			
			 ISO 2039-1 
			 | 
		|
| 
			 Pencil Hardness test, 1kgf 
			 | 
			
			 H 
			 | 
			
			 - 
			 | 
			
			 ASTM D 3363 
			 | 
		|
| 
			 Erichson scratch depth, 6N 
			 | 
			
			 14 
			 | 
			
			 micrometer 
			 | 
			
			 SABIC Method 
			 | 
		|
| 
			 IMPACT 
			 | 
			Value | Unit | Standard | |
| 
			 Izod Impact, unnotched, 23°C 
			 | 
			
			 NB 
			 | 
			
			 cm-kgf/cm 
			 | 
			
			 ASTM D 4812 
			 | 
		|
| 
			 Izod Impact, notched, 23°C 
			 | 
			
			 3 
			 | 
			
			 cm-kgf/cm 
			 | 
			
			 ASTM D 256 
			 | 
		|
| 
			 Izod Impact, notched, -30°C 
			 | 
			
			 3 
			 | 
			
			 cm-kgf/cm 
			 | 
			
			 ASTM D 256 
			 | 
		|
| 
			 Instrumented Impact Total Energy, 23°C 
			 | 
			
			 305 
			 | 
			
			 cm-kgf 
			 | 
			
			 ASTM D 3763 
			 | 
		|
| 
			 Izod Impact, unnotched 80*10*3 +23°C 
			 | 
			
			 NB 
			 | 
			
			 kJ/m2 
			 | 
			
			 ISO 180/1U 
			 | 
		|
| 
			 Izod Impact, unnotched 80*10*3 -30°C 
			 | 
			
			 45 
			 | 
			
			 kJ/m2 
			 | 
			
			 ISO 180/1U 
			 | 
		|
| 
			 Izod Impact, notched 80*10*3 +23°C 
			 | 
			
			 5 
			 | 
			
			 kJ/m2 
			 | 
			
			 ISO 180/1A 
			 | 
		|
| 
			 Izod Impact, notched 80*10*3 -30°C 
			 | 
			
			 4 
			 | 
			
			 kJ/m2 
			 | 
			
			 ISO 180/1A 
			 | 
		|
| 
			 Charpy 23°C, V-notch Edgew 80*10*3 sp=62mm 
			 | 
			
			 3 
			 | 
			
			 kJ/m2 
			 | 
			
			 ISO 179/1eA 
			 | 
		|
| 
			 Charpy -30°C, V-notch Edgew 80*10*3 sp=62mm 
			 | 
			
			 3 
			 | 
			
			 kJ/m2 
			 | 
			
			 ISO 179/1eA 
			 | 
		|
| 
			 Charpy 23°C, Unnotch Edgew 80*10*3 sp=62mm 
			 | 
			
			 NB 
			 | 
			
			 kJ/m2 
			 | 
			
			 ISO 179/1eU 
			 | 
		|
| 
			 Charpy -30°C, Unnotch Edgew 80*10*3 sp=62mm 
			 | 
			
			 47 
			 | 
			
			 kJ/m2 
			 | 
			
			 ISO 179/1eU 
			 | 
		|
| 
			 THERMAL 
			 | 
			Value | Unit | Standard | |
| 
			 Vicat Softening Temp, Rate B/50 
			 | 
			
			 139 
			 | 
			
			 °C 
			 | 
			
			 ASTM D 1525 
			 | 
		|
| 
			 HDT, 0.45 MPa, 3.2 mm, unannealed 
			 | 
			
			 133 
			 | 
			
			 °C 
			 | 
			
			 ASTM D 648 
			 | 
		|
| 
			 HDT, 1.82 MPa, 3.2mm, unannealed 
			 | 
			
			 119 
			 | 
			
			 °C 
			 | 
			
			 ASTM D 648 
			 | 
		|
| 
			 CTE, -40°C to 95°C, flow 
			 | 
			
			 7.E-05 
			 | 
			
			 1/°C 
			 | 
			
			 ASTM E 831 
			 | 
		|
| 
			 CTE, -40°C to 95°C, xflow 
			 | 
			
			 7.E-05 
			 | 
			
			 1/°C 
			 | 
			
			 ASTM E 831 
			 | 
		|
| 
			 Specific Heat 
			 | 
			
			 1.4 
			 | 
			
			 J/g-°C 
			 | 
			
			 ASTM C 351 
			 | 
		|
| 
			 Thermal Conductivity 
			 | 
			
			 0.2 
			 | 
			
			 W/m-°C 
			 | 
			
			 ASTM C 177 
			 | 
		|
| 
			 Thermal Conductivity 
			 | 
			
			 0.2 
			 | 
			
			 W/m-°C 
			 | 
			
			 ISO 8302 
			 | 
		|
| 
			 CTE, 23°C to 80°C, flow 
			 | 
			
			 7.E-05 
			 | 
			
			 1/°C 
			 | 
			
			 ISO 11359-2 
			 | 
		|
| 
			 CTE, 23°C to 80°C, xflow 
			 | 
			
			 7.E-05 
			 | 
			
			 1/°C 
			 | 
			
			 ISO 11359-2 
			 | 
		|
| 
			 Ball Pressure Test, 125°C +/- 2°C 
			 | 
			
			 Passes 
			 | 
			
			 - 
			 | 
			
			 IEC 60695-10-2 
			 | 
		|
| 
			 Ball Pressure Test, approximate maximum 
			 | 
			
			 140 
			 | 
			
			 °C 
			 | 
			
			 IEC 60695-10-2 
			 | 
		|
| 
			 Vicat Softening Temp, Rate B/50 
			 | 
			
			 138 
			 | 
			
			 °C 
			 | 
			
			 ISO 306 
			 | 
		|
| 
			 Vicat Softening Temp, Rate B/120 
			 | 
			
			 140 
			 | 
			
			 °C 
			 | 
			
			 ISO 306 
			 | 
		|
| 
			 HDT/Bf, 0.45 MPa Flatw 80*10*4 sp=64mm 
			 | 
			
			 131 
			 | 
			
			 °C 
			 | 
			
			 ISO 75/Bf 
			 | 
		|
| 
			 HDT/Af, 1.8 MPa Flatw 80*10*4 sp=64mm 
			 | 
			
			 118 
			 | 
			
			 °C 
			 | 
			
			 ISO 75/Af 
			 | 
		|
| 
			 PHYSICAL 
			 | 
			Value | Unit | Standard | |
| 
			 Specific Gr***ity 
			 | 
			
			 1.2 
			 | 
			
			 - 
			 | 
			
			 ASTM D 792 
			 | 
		|
| 
			 Specific Volume 
			 | 
			
			 0.85 
			 | 
			
			 cm2g 
			 | 
			
			 ASTM D 792 
			 | 
		|
| 
			 Density 
			 | 
			
			 1.17 
			 | 
			
			 g/cm2 
			 | 
			
			 ASTM D 792 
			 | 
		|
| 
			 Water Absorption, 24 hours 
			 | 
			
			 0.08 
			 | 
			
			 % 
			 | 
			
			 ASTM D 570 
			 | 
		|
| 
			 Water Absorption, equilibrium, 23C 
			 | 
			
			 0.28 
			 | 
			
			 % 
			 | 
			
			 ASTM D 570 
			 | 
		|
| 
			 Water Absorption, 50% RH, equilib 
			 | 
			
			 0.13 
			 | 
			
			 % 
			 | 
			
			 ASTM D 570 
			 | 
		|
| 
			 Moisture Absorption, 50% RH, 24 hrs 
			 | 
			
			 0.04 
			 | 
			
			 % 
			 | 
			
			 ASTM D 570 
			 | 
		|
| 
			 Mold Shrinkage, flow, 3.2 mm 
			 | 
			
			 0.5 - 0.8 
			 | 
			
			 % 
			 | 
			
			 SABIC Method 
			 | 
		|
| 
			 Melt Flow Rate, 300°C/1.2 kgf 
			 | 
			
			 14.5 
			 | 
			
			 g/10 min 
			 | 
			
			 ASTM D 1238 
			 | 
		|
| 
			 Density 
			 | 
			
			 1.17 
			 | 
			
			 g/cm2 
			 | 
			
			 ISO 1183 
			 | 
		|
| 
			 Water Absorption, (23°C/sat) 
			 | 
			
			 0.27 
			 | 
			
			 % 
			 | 
			
			 ISO 62 
			 | 
		|
| 
			 Moisture Absorption (23°C / 50% RH) 
			 | 
			
			 0.13 
			 | 
			
			 % 
			 | 
			
			 ISO 62 
			 | 
		|
| 
			 Melt Volume Rate, MVR at 300°C/1.2 kg 
			 | 
			
			 13 
			 | 
			
			 cm210 min 
			 | 
			
			 ISO 1133 
			 | 
		|
| 
			 FLAME CHARACTERISTICS 
			 | 
			Value | Unit | Standard | |
| 
			 UL Recognized, 94V-2 Flame Class Rating (3) 
			 | 
			
			 1 
			 | 
			
			 mm 
			 | 
			
			 UL 94 
			 | 
		|
| 
			 UL Recognized, 94V-0 Flame Class Rating (3) 
			 | 
			
			 1.5 
			 | 
			
			 mm 
			 | 
			
			 UL 94 
			 | 
		|

如果您对我们的Lexan PC DMX9455有任何疑问,或者想索取Lexan PC DMX9455 物性表datasheet、物质安全资料证书MSDS、ROHS检验报告、SGS报告、REACH环保证明、FDA证明、EU证明、UL证书及出厂证明COC/COA报告等,敬请拨打我们的服务电话,或者点击 联系我们 给我们留言。