Atom Arc T was developed for welding T-1 steel in all applicati***. Mechanical properties of the welded joints equal or exceed the properties of the base steel in either the as welded or stress relieved condition, thus giving 100% design joint efficiency. In addition, Atom Arc T electrodes are suitable for many other applicati***, particularly where high-strength welds with excellent low temperature impact properties are required.
Typical Tensile Properties
| Condition | Elongation | Stress Relieved Temperature | Stress Relieved Testing Time | Tensile Strength | Yield Strength | 面积缩小 |
| Stress Relieved | 23 % | 1025 °F | 1 hr | 112 ksi | 102 ksi | 62 % |
| As Welded | 23 % | - | - | 115 ksi | 105 ksi | 62 % |
夏比V型缺口冲击性能
| Condition | Impact Value | Testing Temperature | Stress Relieved Testing Temp | Stress Relieved Testing Time |
| As Welded | 55 ft-lb | 0 °F | - | - |
| As Welded | 48 ft-lb | -40 °F | - | - |
| As Welded | 44 ft-lb | -60 °F | - | - |
| Stress Relieved | 50 ft-lb | - | 1025 °F | 1 hr |
| Stress Relieved | 42 ft-lb | - | 1025 °F | 1 hr |
| Stress Relieved | 25 ft-lb | - | 1025 °F | 1 hr |
焊缝金属分析
| P | |||||||
| P | Mn | Mo | C | S | Si | Ni | Cr |
| 0.01 % | - | - | - | - | - | - | - |
| Mn | |||||||
| P | Mn | Mo | C | S | Si | Ni | Cr |
| - | 1.48 % | - | - | - | - | - | - |
| Mo | |||||||
| P | Mn | Mo | C | S | Si | Ni | Cr |
| - | - | 0.38 % | - | - | - | - | - |
| C | |||||||
| P | Mn | Mo | C | S | Si | Ni | Cr |
| - | - | - | 0.05 % | - | - | - | - |
| Si | |||||||
| P | Mn | Mo | C | S | Si | Ni | Cr |
| - | - | - | - | - | 0.30 % | - | - |
| Ni | |||||||
| P | Mn | Mo | C | S | Si | Ni | Cr |
| - | - | - | - | - | - | 1.95 % | - |
| Cr | |||||||
| P | Mn | Mo | C | S | Si | Ni | Cr |
| - | - | - | - | - | - | - | 0.24 % |