OK Tigrod 5754 is a solid aluminium rod with a content of 3% Mg. It is recommended for welding of Al-Mg alloys with less than 3% magnesium. The alloy has a relatively high strength and corrosion resistance.
Typical Tensile Properties
| As welded | ||
| Elongation | Tensile Strength | Yield Strength |
| 23 % | 230 MPa | 110 MPa |
焊缝金属分析
| Mn | ||||||||
| Mn | Cu | Zn | Ti | Si | Mg | Al | Cr | Fe |
| 0.26 % | - | - | - | - | - | - | - | - |
| Cu | ||||||||
| Mn | Cu | Zn | Ti | Si | Mg | Al | Cr | Fe |
| - | 0.01 % | - | - | - | - | - | - | - |
| Zn | ||||||||
| Mn | Cu | Zn | Ti | Si | Mg | Al | Cr | Fe |
| - | - | 0.01 % | - | - | - | - | - | - |
| Ti | ||||||||
| Mn | Cu | Zn | Ti | Si | Mg | Al | Cr | Fe |
| - | - | - | 0.13 % | - | - | - | - | - |
| Si | ||||||||
| Mn | Cu | Zn | Ti | Si | Mg | Al | Cr | Fe |
| - | - | - | - | 0.03 % | - | - | - | - |
| Mg | ||||||||
| Mn | Cu | Zn | Ti | Si | Mg | Al | Cr | Fe |
| - | - | - | - | - | 3.1 % | - | - | - |
| Al | ||||||||
| Mn | Cu | Zn | Ti | Si | Mg | Al | Cr | Fe |
| - | - | - | - | - | - | 96.19 % | - | - |
| Cr | ||||||||
| Mn | Cu | Zn | Ti | Si | Mg | Al | Cr | Fe |
| - | - | - | - | - | - | - | 0.15 % | - |
| Fe | ||||||||
| Mn | Cu | Zn | Ti | Si | Mg | Al | Cr | Fe |
| - | - | - | - | - | - | - | - | 0.09 % |