适用于焊接29% Cr-9% Ni牌号材料的抗腐蚀铬镍焊丝。OK Tigrod 312由于铬含量较高,在高温条件下具有良好的***化性。该合金广泛用于焊接异种钢材,尤其是其中一方为全奥氏体的异种钢焊接,也适用于诸如设备组件、刀具、奥氏体锰钢等难以焊接的钢材。
Typical Tensile Properties
| As welded | ||
| Elongation | Tensile Strength | Yield Strength |
| 20 % | 770 MPa | 610 MPa |
夏比V型缺口冲击性能
| As welded | |
| Impact Value | Testing Temperature |
| 50 J | 20 °C |
焊缝金属分析
| Mn | ||||||
| Mn | Mo | Cu | C | Si | Ni | Cr |
| 1.6 % | - | - | - | - | - | - |
| Mo | ||||||
| Mn | Mo | Cu | C | Si | Ni | Cr |
| - | 0.20 % | - | - | - | - | - |
| Cu | ||||||
| Mn | Mo | Cu | C | Si | Ni | Cr |
| - | - | 0.14 % | - | - | - | - |
| C | ||||||
| Mn | Mo | Cu | C | Si | Ni | Cr |
| - | - | - | 0.10 % | - | - | - |
| Si | ||||||
| Mn | Mo | Cu | C | Si | Ni | Cr |
| - | - | - | - | 0.4 % | - | - |
| Ni | ||||||
| Mn | Mo | Cu | C | Si | Ni | Cr |
| - | - | - | - | - | 8.8 % | - |
| Cr | ||||||
| Mn | Mo | Cu | C | Si | Ni | Cr |
| - | - | - | - | - | - | 30.7 % |